QUARTER PANEL > CUT AND JOIN REPLACEMENT SECTIONS (SMALL AREAS) | |
- Quarter Panel Replacement Using Adhesive
Work Procedure
- Cut the wheel arch portion.
- Heat the quarter panel adhesive area and remove the quarter panel.
- HINT:
- Using an industrial heater gun or gas burner, heat the quarter panel to 110 to 140°C. Make sure the quarter panel does not warp.
- Clean off any adhesive that remains on the vehicle.
- HINT:
- Using an industrial heater gun or gas burner, heat the adhesive to 110 to 140°C.
- Using a scraper, scrape away the adhesive.
- If adhesive remains, the strength of any subsequently applied adhesive will be weak.
- Using a disc grinder or belt sander, scuff and sand any adhesive that remains on the vehicle.
- HINT:
- Scuff at a width of approximately 10 mm (0.39 in.) over the previous adhesive coating.
- Apply adhesive to the exposed metal areas on the vehicle. Using a spatula, spread the adhesive evenly.
- Apply adhesive to the vehicle again.
- Using #60-120 grit sandpaper, scuff the adhesive application area on the new quarter panel.
- Apply adhesive to the new quarter panel. Using a spatula, spread the adhesive evenly.
- Using a vise grip or the palms of your hands, press the quarter panel so that the thickness of the adhesive is even.
- Complete installation the new quarter panel.
- Dry the adhesive areas of the new quarter panel.
- HINT:
- With dryer or equivalent (60°C): 60 minutes (complete hardening: 90 minutes)
- Ambient temperature (25°C): 12 hours (complete hardening: 24 hours)
Symbol meaning
|

| Remove Weld Points
|

| Cut and Join Location
|

| Cut Location for Supply Parts
|
REMOVAL POINT (for TMC, TMMR Made)
- *1 in illustration above indicates where the adhesive is located.
- Roughly cut open the panel so that the adhesive can be reached. Cut through the adhesive with a cut chisel to remove the panel.
- HINT:
- In cases where the adhesive cannot be removed with a cut chisel, heat the adhesive with an industrial heater gun or gas burner taking care not to cause panel deformation by overheating.
REMOVAL POINT (for TMMK Made)
- After grinding off the hemming location, remove the quarter panel.
- *1 in illustration above indicates where the adhesive is located.
- Roughly cut open the panel so that the adhesive can be reached. Cut through the adhesive with a cut chisel to remove the panel.
- HINT:
- In cases where the adhesive cannot be removed with a cut chisel, heat the adhesive with an industrial heater gun or gas burner taking care not to cause panel deformation by overheating.
Symbol meaning
|

| Spot Weld
|

| Plug Weld
|

| Butt Weld
|
INSTALLATION POINT (for TMC, TMMR Made)
- Inspect the fitting of the related parts around the new parts before welding. This affects the appearance of the finish.
- Temporarily install the new parts and measure each part of the new parts in accordance with the body dimension diagram. (See the body dimension diagram)
- Apply adhesive (3MTM AutomixTM Panel Bonding Adhesive #8115) to the area indicated by *1 in the illustration.
- HINT:
- Apply enough adhesive for the panels to stick to each other.
- After welding, apply body sealer to the corresponding parts. (See the painting / coating)
- After applying the top coat, apply anti-rust agent to the internal panel portion of the closed section structural weld points.
INSTALLATION POINT (for TMMK Made)
- Inspect the fitting of the related parts around the new parts before welding. This affects the appearance of the finish.
- Temporarily install the new parts and measure each part of the new parts in accordance with the body dimension diagram. (See the body dimension diagram)
- After welding, apply the foamed sealing material to the corresponding parts. (See the painting /coating)
- Bend the flange hem with a wooden hammer and dolly.
- HINT:
- Bend the panel gradually so as not to distort it.
- Apply adhesive (3MTM AutomixTM Panel Bonding Adhesive #8115) to the area indicated by *1 in the illustration.
- HINT:
- Apply enough adhesive for the panels to stick to each other.
- After welding, apply body sealer to the corresponding parts. (See the painting / coating)
- After applying the top coat, apply anti-rust agent to the internal panel portion of the closed section structural weld points.