CONSTRUCTION
Anti-corrosion Sheet Steel
Aluminum and anti-corrosion sheet steel is used as in the following illustration:
| *a | Aluminum | *b | Anti-corrosion Sheet Steel |
| *a | Anti-corrosion Sheet Steel | - | - |
Anti-chipping Application and Rust-resistant Performance
Wax is applied to the edge of the door lower portion, door hinge, fuel filler lid hinge, and the hemmed portions of the hood panel and luggage compartment door panel sub-assembly to improve rust-resistant performance.
| *1 | Hood Hinge Assembly LH | *2 | Hood Hinge Assembly RH |
| *3 | Hood Sub-assembly | *4 | Front Door Hinge Assembly Upper LH |
| *5 | Front Door Hinge Assembly Lower LH | *6 | Rear Door Hinge Assembly Lower LH |
| *7 | Rear Door Hinge Assembly Upper LH | *8 | Back Door Hinge Assembly |
| *9 | Fuel Filler Opening Lid Assembly | - | - |
| *a | A View | *b | B View |
| *c | C - C Cross Section | *d | Wax |
| *e | Anti-chipping Coat (Models for Europe) | - | - |
Polyvinyl Chloride (PVC) coating is applied to the wheel housings, and other parts that are located where they are susceptible to stone chipping damage, improving the rust-resistance of these areas.
| *A | LHD Models | *B | RHD Models |
| *a | Edge Seal | *b | Under Coating Area (All Dest.) |
| *c | Under Coating Area (Models for Europe and destination package for Korea) | - | - |
| *A | LHD Models | *B | RHD Models |
| *a | Edge Seal | *b | Under Coating Area (All Dest.) |
| *c | Under Coating Area (Models for Europe, Russia and destination package for Korea) | - | - |