INTRODUCTION  WORK NOTICES AND PRECAUTIONS  PRECAUTIONS FOR WELDING  


REMOVAL OF ADJACENT COMPONENTS


a.
K110072

To prevent damage to the body and parts, apply protective tape to the body and tools before removing the parts.

NOTICE:

If the paint film is damaged, make sure to refinish the paint.




CUTTING WORK


K110073

a.

When cutting a panel, be careful not to damage the surrounding panels or any panels underneath.

NOTICE:

If any panels are damaged, be sure to repair them.




ANTI-RUST TREATMENT BEFORE WELDING


a.
K110074

Apply welding primer to the contact surfaces of the welding areas to protect them from rust.

NOTICE:

Do not apply welding primer outside of the contact surfaces.




WELDING WORK


a.
K110075C08
1.104,0.927 1.552,0.656 1.552,0.656 1.719,0.656 true 1.771,0.594 2.083,0.844 0.313,0.25 10 false *a
*a 1500 MPa or 1180 MPa or 980 MPa or 780 MPa ultra high strength steel


K110076C08
1.052,0.938 1.552,0.625 1.552,0.625 1.729,0.625 true 1.781,0.563 2.094,0.802 0.313,0.24 10 false *a
*a 1500 MPa or 1180 MPa or 980 MPa or 780 MPa ultra high strength steel


Follow the welding conditions below when welding ultra high strength steel to assure sufficient weld strength.

When welding 2 panels together including 1500 MPa or 1180 MPa or 980 MPa or 780 MPa ultra high strength steel.
Plug weld Plug diameter 8 mm (0.31 in.)
Wire type AWS A5.18 ER70S-3
Shield gas Metal active gas

NOTICE:

Be sure to use Metal active gas (Ar 80% + CO2 20%) as the shield gas when plug welding. Sufficient weld strength cannot be assured when using 100% CO2 shield gas.


When welding more than 3 panels together including 1500 MPa or 1180 MPa or 980 MPa or 780 MPa ultra high strength steel. (When plug welding a third panel to 2 panels which are welded under the conditions described above.)
Plug weld Plug diameter Same as the standard method
(See the introduction)
Wire type AWS A5.18 ER70S-3
Shield gas Metal active gas

NOTICE:

Be sure to use Metal active gas (Ar 80% + CO2 20%) as the shield gas when plug welding. Sufficient weld strength cannot be assured when using 100% CO2 shield gas.



b.

Standard Number of Welds

Number of plug welds 1180 MPa or 980 MPa or 780 MPa ultra high strength steel More than the number of welds made by the manufacturer
Normal steel or high strength steel



PRECAUTION WHEN REPLACING WELDED PANELS WITH ADHESIVE


a.

When using welds to attach panels that were previously attached using adhesive, it must be welded by plug welding (MAG welding), no adhesive should be applied. The number of plug welds (MAG welding) must be doubled compared to the original welding points on the adhesive applied areas.



MAKING HOLES FOR PLUG WELDING


K110078C02
1.396,1.896 1.573,1.896 1.573,1.896 2.021,1.625 false 1.146,1.802 1.458,2.104 0.313,0.302 10 false *a
*a Puncher


a.

For areas where a spot welder cannot be used, use a puncher or drill to make holes for plug welding.

Thickness of Welded Portion Diameter of Plug Hole
Under 1.0 mm (0.04 in.) Over 5.0 mm (0.20 in.)
1.0 to 1.6 mm (0.04 to 0.06 in.) Over 6.5 mm (0.26 in.)
1.7 to 2.3 mm (0.07 to 0.09 in.) Over 8.0 mm (0.31 in.)
Over 2.4 mm (0.09 in.) Over 10 mm (0.39 in.)