REMOVAL
| Symbol Meaning | |
|---|---|
|
Remove Weld Points |
|
Remove Weld Points |
|
Cut and Join Location |
|
Cut Location for Supply Parts |
Do not butt weld or heat repair because the heat decreases the strength of areas where ultra high strength steel is used. (See the introduction)
Remove the center body pillar outer.
| *a | 20 mm (0.79 in.) | - | - |
| *1 | CENTER BODY PILLAR OUTER | - | - |
| *a | 160 mm (6.30 in.) | - | - |
Remove the center body pillar reinforcement sub-assembly.
| *1 | CENTER BODY PILLAR REINFORCEMENT SUB-ASSEMBLY | - | - |
After removing the A, remove the center body pillar reinforce sub-assembly lower.
| *1 | CENTER BODY PILLAR REINFORCE SUB-ASSEMBLY LOWER | - | - |
| *a | 20 mm (0.79 in.) | *b | 55 mm (2.17 in.) |
INSTALLATION
| Symbol Meaning | |
|---|---|
|
Remove Weld Points |
|
Remove Weld Points |
|
Plug Weld |
|
Plug Weld |
|
Cut and Join Location |
|
Butt Weld |
Inspect the fitting of the related parts around the new parts before welding. This affects the appearance of the finish.
Temporarily install the new parts and measure each part of the new parts in accordance with the body dimension diagram. (See the body dimensions)
If the entire supply part is not needed, remove the part of the supply part that is needed.
A is reused.
| *1 | CENTER BODY PILLAR REINFORCE SUB-ASSEMBLY LOWER | - | - |
| *a | 20 mm (0.79 in.) | *b | 55 mm (2.17 in.) |
After welding the center body pillar reinforce sub-assembly lower to the vehicle, install the A.
| *1 | CENTER BODY PILLAR REINFORCE SUB-ASSEMBLY LOWER | - | - |
Weld the center body pillar reinforcement sub-assembly to the vehicle side.
| *1 | CENTER BODY PILLAR REINFORCEMENT SUB-ASSEMBLY | - | - |
| *a | Ultra High Strength Steel Welding Point | - | - |
When welding 2 panels together including 1500 MPa ultra high strength steel.
| *a: Plug weld | Plug diameter | 10 mm (0.39 in.) |
| Wire type | AWS A5.18 ER70S-6/ER70S-3 | |
| Shield gas | Metal active gas |
Be sure to use Metal active gas (Ar + CO2 20 to 30% or Ar + O2 2%) as the shield gas when plug welding. Sufficient weld strength cannot be assured when using 100% CO2 shield gas.
Weld the center body pillar outer to the vehicle side.
| *1 | CENTER BODY PILLAR OUTER | - | - |
| *a | Ultra High Strength Steel Welding Point | - | - |
When welding 3 panels or more together including 1500 MPa ultra high strength steel. (When plug welding a third panel to 2 panels which are welded under the conditions described above.)
| *a: Plug weld | Plug diameter | Same as the standard method (See the introduction) |
| Wire type | AWS A5.18 ER70S-6/ER70S-3 | |
| Shield gas | Metal active gas |
Be sure to use Metal active gas (Ar + CO2 20 to 30% or Ar + O2 2%) as the shield gas when plug welding. Sufficient weld strength cannot be assured when using 100% CO2 shield gas.
After welding, apply the foamed sealing material to the corresponding parts. (See the painting/coating)
After welding, apply body sealer to the corresponding parts. (See the painting/coating)
After applying the top coat, apply anti-rust agent to the internal panel portion of the closed section structural weld points.